Cold Rolled Steel Sheet DC01 Cold-rolled Steel Plate

It is a non-alloy cold-rolled steel with very low carbon content. It is often used in the automotive industry and for making electronic components. The low carbon content of this steel makes it very easy to work with. It can be welded, brazed and soldered without any issues.

produkt introduktion

produkt introduktion

 

DC01 represents the basic grade of the DC steel family and is also known under the former designations St12 or FeP01. This grade can be used for simple forming operations such as bending, coining, beading and drawing.

JIS G3141,DIN1623,EN10130
SPCC, SPCD SPCE,Q195,DC01,DC02,DC03,DC04,ST12
0.13-3 mm
20-1500 mm,Normal width is 914/1000/1219/1250/1500 mm
General, bright, dull and mirror finish, oiled or non-oiled
508 mm/610 mm
3-12 tons
ISO9001:2008,SGS
Within 10-15 workdays,25-30 days when the quantity beyond 1000 tons.

After cold rolling, it is annealed (continuous or batch process) and skin passed to produce a formable product with a high quality surface finish. Here at John Tainton, we stock and process DC01 mild steel (often referred to as CR4), in varying thicknesses from 0.9mm up to 3mm.

A:(1)One is 30% deposit by TT before production and 70% balance against copy of B/L;
(2)the other is Irrevocable L/C 100% at sight. Q: Can we visit your factory?

 

Cold Rolled Steel Sheet DC01 cold-rolled steel plate

Cold Rolled Steel Sheet DC01 cold-rolled steel plate

Populära Taggar: cold rolled steel sheet dc01 cold-rolled steel plate, China cold rolled steel sheet dc01 cold-rolled steel plate manufacturers, suppliers, factory, Galvaniserade stålförpackningsartiklar, Galvaniserade stållagringar, galvaniserad stålimportör

Skicka förfrågan

Skicka förfrågan