Produktnamn
|
Galvaniserad stålspole, galvaniserad stålspole, zinkbelagd stålspole, GI, HDGI
GalValume Steel Coil, Aluzinc Steel Coil, Zink Aluminium Steel Coil, GL, HDGL
|
|
Standard
|
EN10147, EN10142, DIN 17162, JIS G3302, ASTM A653
|
|
Stålklass
|
DX51D, DX52D, DX53D, DX54D, S220GD, S250GD, S280GD, S350GD, S350GD,
S550GD; SGCC, SGHC, SGCH, SGH340, SGH400, SGH440, SGH490, SGH540, SGCD1, SGCD2, SGCD3, SGC340, SGC340, SGC490, SGC570; SQ CR22 (230), SQ CR22 (255), SQ CR40 (275), SQ CR50 (340), SQ CR80 (550), CQ, FS, DDS, EDDS, SQ CR33 (230), SQ CR37 (255), SQCR40 (275), SQ CR50 (340 (340, CREQ CR350; eller som krav
|
|
Typ
|
Spole/plåt/remsa
|
|
Material
|
CGCC/SGCH/G350/G450/G550/DX51D/DX52D/DX53D
|
|
Tjocklek
|
{{0}}. 12mm -4. 0 mm eller 0. 8mm/1. 0 mm/1.2mm/1.5mm/2.0mm
|
|
Bredd
|
600mm -1500 mm eller 914mm/1000mm/1200mm/1219mm/1220mm
|
|
Zinkbeläggning
|
Z30g/m2-Z350g/m2
|
|
Ytstruktur
|
Normal spanglebeläggning (NS), minimerad spanglebeläggning (MS), spangle-fri (FS)
|
|
Spolvikt
|
3 ton -8 ton
|
|
Spole ID
|
508mm/610mm
|

Efter att det heta galvaniserade stålplåten dras ut ur zinkpotten kallas utseendet på kristallkornen som zinkskiktet svalnar och stelnar spangles. Storleken, ljusstyrkan och ytmorfologin hos spangles beror på en serie faktorer, men de är främst relaterade till sammansättningen av zinkskiktet och kylmetoden. Galvaniserad stålspole har fördelarna med enhetlig beläggning, stark vidhäftning och lång livslängd.

Populära Taggar: DX51D galvaniserad kall rullad rostfritt stålspole DC01, Kina DX51D galvaniserad kall rullad rostfritt stålspole DC01 Tillverkare, leverantörer, fabrik, Galvaniserade stålskärningstillbehör, galvaniserad stålimportör, Galvaniserade stålförpackningsartiklar, Galvaniserade stållagringar, galvaniserad stål grossist, galvaniserad ståltråd