Hem-Kunskap-

Innehåll

Cold Rolled Steel Coil Specification DC01 DC03 DC04 DC05 DC06 DC07

Oct 09, 2025

Cold-rolled steel coils

 


Cold-rolled steel coils are steel products that have undergone a cold rolling process. Cold rolling is a manufacturing process in which hot-rolled steel is passed through rollers at room temperature, compressing and shaping it into thinner and more precise coils.

During cold rolling, the hot-rolled steel is first pickled to remove any scale or impurities on the surface. It is then passed through a series of rollers that apply pressure, reducing the thickness of the steel and improving its surface finish. This process also increases the strength and hardness of the steel.


supplies Cold Rolled Steel Coil Product suitable for wide Applications, main standard include JIS G3141, EN10130, EN10268, GB/T5213.
Cold rolled steel coil can be slit into any size with a width of <=1430mm(coil slit) according to customer's requirements; it can also be uncoiled and cut to length(cold rolled steel sheet) ,
our steel mill is equipped with high class uncoiling and straightening production line to guarantee the product quality. Custom package is also available.

 

Cold-Rolled Steel Coils SPCC SPCD SPCE

 

SPCC,SPCD,SPCE,Q195,Q235,DC03,DC04,DC05,HC260LA,HC380LA,HC420LA,HC260P,HC300P,HC260Y
Thickness: 0.5~2.0mm; width: 800-1430mm

JIS G3141, EN10130, EN10268, GB/T5213

 

 

: DC01,DC03,DC04,DC05

: HC260LA,HC380LA,HC420LA

(containing P): HC300P

: HC260Y

 

Cold-Rolled Steel Coils SPCC SPCD SPCE

 

The surface is allowed to have a small amount of defects that do not affect the formability and coating and plating adhesion, such as slight scratches, indentations, pitting, roll marks, and oxidized colors.
The better side of the two sides of the product has no visible defects visible to the naked eye, and the other side should at least meet the requirements of FB.
The better side of the two sides of the product should not have defects affecting the appearance quality after painting or the appearance quality after plating, and the other side should at least meet the requirements of FB.

 

 

  • GB/T5213-2008 Application:

DC01
DC03
DC04
DC05
DC06
DC07

 

  • JIS G3141 Equivalent Steel Grade:

GB/T5213-2008 EN 10130-2006 JIS G3141-2005 ISO 3574-1999 ASTM A1008M-07
DC01 DC01 CR1
DC03 DC03 CR2
DC04 DC04 CR3
DC05 DC05 CR4
DC06 DC06 CR5
DC07 DC07 - - -

 